Abstract
Laser powder bed fusion (L-PBF) was used to produce stator half-shells of a transverse flux machine from pure iron (99.9% Fe). In order to reduce iron losses in the bulk components, radially extending slits with a nominal width of 150 and 300 µm, respectively, were integrated during manufacturing. The components were subjected to a suitable heat treatment. In addition to a microscopic examination of the slit quality, the iron losses were also measured using both a commercial and a self-developed measurement setup. The investigations showed the iron losses can be reduced by up to 49% due to the integrated slits and the heat treatment.