Abstract
SAPO-34 nanocrystals with sizes of 50–150 nm were obtained via steam-assisted crystallization (SAC) for 5 h at 200 °C from two types of aluminum precursors—aluminum isopropoxide and boehmite. A reaction mixture composition with a small amount of organic template tetraehylammonium hydroxide (TEAOH) was used with the molar ratio TEAOH/Al2O3 = 1/1. The alumina precursor type and duration of the SAC (5 and 24 h) on the crystal size, texture, and acid properties were investigated. The SAPO-34 nanocrystals that we obtained possess a large micropore volume of 0.22–0.24 cm3/g and a specific surface area of 651–695 m2/g. When the crystallization was prolonged for up to 24 h, a SAPO-18 structure appeared, but the micropore and mesopore volumes changed insignificantly. Using boehmite as the aluminum precursor led to higher mesoporosity of the material but a little bit lower acidity when compared with the samples prepared from aluminum isopropoxide. In addition, the method proposed was used for preparing a SAPO-34-coated aluminum adsorber heat exchanger. Thus, the synthesis method proposed is affordable and effective to prepare SAPO-34 highly crystalline nanoparticles, with no need for post-synthetic procedures as the mother liquor separation from nanocrystals.
Funder
Russian Science Foundation
Subject
General Materials Science,General Chemical Engineering
Reference42 articles.
1. Aluminophosphate Molecular Sieves and the Periodic Table;Stud. Surf. Sci. Catal.,1986
2. Baerlocher, C., McCusker, L.B., and Olson, D.H. (2007). Atlas of Zeolite Framework Types, Elsevier. [6th ed.].
3. Recent Progress in the Selective Catalytic Reduction of NO with NH3 on Cu-SAPO-34 Catalysts;Mol. Catal.,2022
4. Role of Texture and Acidity of SAPO-34 in Methanol to Olefins Conversion;Pet. Chem.,2020
5. Methanol to Olefins (MTO): From Fundamentals to Commercialization;ACS Catal.,2015
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献