AbstractCr‐free paints applied on different aluminum alloys were exposed for 5 years at different atmospheric weathering sites worldwide. By image analysis, the extent, and the type of corrosion (filiform or blistering) were determined after 1, 2, and 5 years. In that way, it was possible to rank the different systems as a function of their resistance to corrosion. The kinetics of degradation of each system at all sites was also determined. From the results, it is shown that the kinetics of degradation is system dependent. It is also shown that it is the combination of several climatic parameters which contributes to the corrosivity of the site and not only one single parameter such as chloride deposition, relative humidity, and so on.
Subject
Materials Chemistry,Metals and Alloys,Surfaces, Coatings and Films,Mechanical Engineering,Mechanics of Materials,Environmental Chemistry,Materials Chemistry,Metals and Alloys,Surfaces, Coatings and Films,Mechanical Engineering,Mechanics of Materials,Environmental Chemistry,Materials Chemistry,Metals and Alloys,Surfaces, Coatings and Films,Mechanical Engineering,Mechanics of Materials,Environmental Chemistry
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献