1. W.W. Love et al., The use of Ti-38644 titanium for downhole production casing in geothermal wells, 6th World Conf. Titanium Proceedings, Cannes, Soc. Francaise Metall., 1988, pp. 443–448.
2. R.W. Schutz, M. Xiao, T.A. Bednarowicz, Stress corrosion behavior of the Ti–3Al–8V–6Cr–4Zr–4Mo titanium under deep sour gas well conditions, Corrosion 1992, 51, NACE, Houston, TX, 1992.
3. D.R. Klink, R.W. Schutz, Engineering incentives for utilizing Ti–3Al–8V–6Cr–4Zr–4Mo titanium tubulars in highly aggressive deep sour gas wells, Corrosion 1992, 63, NACE, Houston, TX, 1992.
4. R.W. Schutz, M. Xiao, J.W. Skogsberg, Stress cracking and crevice corrosion testing of Pd-enhanced Beta-C™ titanium pipe and billet products in a worst-case sour gas well environment, Proc. 12th Int. Corrosion Congress, vol. 4, NACE, Houston, TX, 1993, p. 2506.
5. R.W. Schutz, S.R. Seagle, Method for Improving Aging Response and Uniformity in β Titanium Alloys, US Patent No. 5 201 967, 1993.