1. Failure analysis of cracked 2.25Cr–1.0Mo steel tubes of an oil refinery boiler;Ahmadi;Engineering Failure Analysis,2020
2. In situ monitoring of crevice corrosion morphology of type 316l stainless steel and re-passivation behavior induced by sulfate ions;Aoyama;Corrosion Science,2017
3. Influence of Thermal Treatment on SCC and HE Susceptibility of Supermartensitic Stainless Steel 16Cr5NiMo;Bacchi;Materials,2020
4. Bagchi, A., Gope, D.K., Chattopadhyaya, S., Wuriti, G., 2020. A critical review on susceptibility of stress corrosion cracking in maraging steel weldments. Materials Today: Proceedings 13, 2303–2307.
5. Bovard, F., Henon, C., Wyss, R., Wong, C., Curran, J., Towers, J., Padrul, J., 2011. Development of test specimens for evaluating SCC behavior of marine aluminum alloys and assessment of the severity of various marine exposure conditions. International Corrosion Conference Series. 1–7.