Abstract
In mechanical engineering, the antifriction tin bronzes, and C92900 bronze for instance are used for parts subjected to wear. The permanent mold casting into steel molds are commonly used to produce parts from C92900 bronze. This work investigates the possibility of C92900 bronze rods production by hot extrusion and upcasting methods. It has been discovered the hot extrusion temperature and ram speed, as well as the casting speed for upcasting that promote no defects in rods. It has been shown that hot extrusion leads to severe grain refinement up to 1.7 gm, and when casting upwards, on the contrary, an increase in the grain size occurs in comparison with the permanent mold casting. After hot extrusion and upcasting, the crystals of the Y-Cu3Sn intermetallic phase are refined in the bronze microstructure. At the same time, large agglomerations of (Pb) particles can be observed in the extruded bronze microstructure, which leads to a decrease in the coefficient of friction. The maximum hardness and tensile strength were obtained for rods produced by hot extrusion at 600 °C, and the highest elongation in rods obtained by the upcasting method. Tribological studies were carried out according to the «shaft — partial insert» scheme in a kerosene medium with a steel counter body showed that hot extrusion leads to a tenfold increase in wear resistance and a threefold decrease in the friction coefficient in comparison with rods obtained by permanent mold casting. At the same time, for the rods obtained by the upcast method, on the contrary, a decrease in wear resistance is observed. In connection with the mentioned results, it is possible to recommend the hot extrusion method for producing C92900 bronze rods in addition with casting technique.
Publisher
National University of Science and Technology MISiS
Reference36 articles.
1. Gruzdeva I.A., Sulitsyn A.V., Mysik R.K., Sokunov B.A. Influence of electromagnetic stirring on the microstructure and properties of tin bronze. Liteishchik Rossii. 2006. No. 11. P. 27—29 (In Russ.).
2. Song K., Zhou Y., Zhao P., Zhang Y., Bai N. Cu—10Sn— 4Ni—3Pb alloy prepared by crystallization under pressure: An experimental study. Acta Metall. Sin. 2013. Vol. 26. P. 199—205.
3. Belov V.D., Gerasimenko E.A., Guseva V.V., Konovalov A.N. Influence of BrO10S2N3 tin bronze solidification conditions on its microstructure. Liteinoe proizvodstvo. 2016. No. 2. P. 26—33 (In Russ.).
4. Ozerdem M.S., Kolukisa S. Artificial neural network approach to predict the mechanical properties of Cu—Sn— Pb—Zn—Ni cast alloys. Mater. Design. 2009. Vol. 30. P. 764—769.
5. Vershinin P.I., Sevast'yanov V.I., Bakrin Yu.N. Influence of cooling intensification on microstructure and properties of tin bronze castings. Liteinoe proizvodstvo. 1986. No. 5. P. 8—9 (In Russ.).