In this work, the high-temperature diffusion doping method was used for introduction of active cobalt ions into calcium orthovanadate Ca3(VO4)2crystals. Experimental samples were made from a nominally pure CVO single crystal obtained by the Czochralski method. The high-temperature diffusion conditions have been optimized to obtain doped crystals of optical quality during annealing in open and closed zones. Diffusion coefficients of cobalt ions (D) were calculated for various conditions: annealing time 24 - 48 hours; temperature range 1150-1300°C; diffusants - oxide compounds of calcium, cobalt and vanadium: Co3O4, Ca10Co0.5(VO4)7 and Ca3(VO4)2:2wt.%Co3O4; diffusion direction is parallel or perpendicular to the CVO crystal optical axis. The calculated values of the diffusion coefficient varied between 2.09·10-8—1.58·10-7 cm2/s. The activation energy of the diffusion process was determined to be 2.58±0.5 and 2.63±0.5 eV for the [001] and [100] directions, respectively. The maximum cobalt concentration in doped CVO crystals was 2·1020 cm–3. The absorption spectrum of diffusion-doped Ca3(VO4)2:Co samples demonstrates the presence of absorption bands characteristic for Co2+ and Co3+ ions. It was shown that the intensity ratio of the characteristic absorption bands varies depending on the crystal doping method. The optical anisotropy of the crystal increases with dopant concentration increase.
Publisher
National University of Science and Technology MISiS