Author:
Negm Samia S. Attia,Moghny A.S. Abdel,Ahmad Syed Ismail
Subject
General Earth and Planetary Sciences,General Environmental Science
Reference43 articles.
1. RT and (b) after annealing at 348 ? 2 K for 1 hr. Microstructure of Sn-8wt.%Zn-2wt.% Bi as-cast (a) at RT and (b) after annealing at 348 ? 2 K for 1 hr. Microstructure of Sn-8wt.%Zn-4wt.% Bi as-cast (a) at RT and (b) after annealing at 348 ? 2 K for 1 hr;RT and (b) after annealing at 348 ? 2 K for 1 hr
2. Comprehensive Composite Materials: Development of Continuously-Reinforced Metal Matrix Composites for Aerospace Applications;P J Doorbar;Comprehensive Composite Materials II,2018
3. Structure and properties of Sn-Cu lead-free solders in electronics packaging;M Zhao;Sci.Tec. Adv. Mater,2019
4. Microstructure formation in Sn-Cu-Ni solder alloys;M Felberbaum;JOM,2011