Based on the CCUS project planned to run in a domestic oil field, the electrochemical corrosion at the bend of supercritical CO2 pipeline was studied by means of high-temperature and high-pressure reaction kettle hanging plate experiment, and the corrosion rate of X80 pipeline steel in unsaturated, saturated and supersaturated supercritical CO2 with water content was obtained. Then through COMSOL simulation of the corrosion rate of 90° bent pipe in the supercritical CO2 corrosion atmosphere, the maximum corrosion rate position of electrochemical corrosion generated under the action of flow accelerated corrosion (FAC) generated by supercritical CO2 fluid in the bent pipe was obtained, and corresponding anticorrosion Suggestions were put forward according to the research results.
Reference18 articles.
1. Development of a facile reclaiming process for degraded alkanolamine and glycol solvents used for CO2 capture systems [J];Ju;International Journal of Greenhouse Gas Control,2018
2. Research Progress in Corrosion of CO2 Conveying Pipeline [J];Hu;Surface Technology,2016
3. Research progress on corrosion of supercritical CO2 transport pipeline containing impurities [J];Sun;Journal of Chinese Society for Corrosion and Protection,2015
4. Discussion of the CO2 corrosion mechanism between low partial pressure and supercritical condition [J];Zhang;Corrosion Science,2012
5. Update of DNV Recommended Practice RP-J202 with Focus on CO2 Corrosion with Impurities [J];Brown;Energy Procedia,2014
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献