Author:
Masnur D,Suyitno ,Malau V
Abstract
Abstract
The influence of mold material on cooling curve, solidification parameters, and micro-hardness were investigated. Al–6wt.% Si in clay and stainless steel mold was directionally solidified using vertical Bridgman type furnace. The samples were heated up to 700°C at 1.9°C/s heat rate, held for 60 minutes, cooled, and withdrawn at 40 µm/s. The results show that the increasing of thermal conductivity by 72% affects cooling curve shape, solidification parameters, and micro-hardness. Furthermore, comparative evaluation of the exponent value of the function of micro-hardness to distance and micro-hardness to growth rate also have been made to proposed the range of exponent value for each mold material.
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献