Author:
Kolosov V N,Miroshnichenko M N,Prokhorova T Yu
Abstract
Abstract
The process of producing W-Cr powders by the reduction of trirutile Cr2WO6 with magnesium vapor in the temperature range 700–850 °C at residual pressure of 5-20 kPa was studied. W-Cr powders with a specific surface area at the level of 43-47 m2⋅g−1 were obtained. The resulting W-Cr powders are characterized by a mesoporous structure.
Subject