1. Liu, Z.G., Guo, J.T., Ye, L.L., Li, G.S., and Hu, Z.Q., Formation mechanism of TiC by mechanical alloying, Appl. Phys. Lett., 1994, vol. 65, no. 21, pp. 2666–2668.
2. Gangler, J.J., Some physical properties of eight refractory oxides and carbides, J. Am. Ceram. Soc., 1950, vol. 33, no. 12, pp. 367–374.
3. Wen, G., Li, S.B., and Zhang, B.S., Reaction synthesis of TiB2–TiC composites with enhanced toughness, Acta Mater., 2001, vol. 49, no. 8, pp. 1463–1470.
4. Chatterjee, S. and Chandrashekhar, S., Deposition methods, properties and metal cutting applications of ceramic films, Key Eng. Mater., 1996, vol. 114, no. 1, pp. 67–104.
5. Yoshiaki, S., Hiroharu, K., Kazuya, D., Jun, N., and Tamiko, O., Preparation of crystalline TiC thin films grown by pulsed YAG:Nd laser deposition using Ti target in methane gas, Mater. Character., 2002, vol. 48, nos. 2–3, pp. 221–228.