Abstract
Abstract
The coefficient of 65Zn heterodiffusion in the Mg17Al12 intermetallic compound (β-phase) and the eutectic alloy Mg-33.4 wt.% Al was measured in the temperature region 598 – 698 K using serial sectioning and residual activity methods. The diffusion coefficient of 65Zn in the intermetallic can be written as Δ
I = 1.5 × 10– 2 m2 s –1 × exp( – 154.3 kJ mol –1/RT). At temperatures T ≥ 648 K, where the mean diffusion path is greater than the mean interlamellar distance in the eutectic, the effective diffusion coefficient Δ
eff = 2.7 × 10– 2 m2 s –1 exp(–155.1 kJ mol– 1/ RT) was evaluated. At two lower temperatures, the diffusion coefficients 65Zn in interphase boundaries were estimated: Δ
b (623 K) = 1.6 × 10 –12 m2 τ– 1 and Δ
b (598 K) = 4.4 × 10– 13 m2 τ–1. The specific (Mg)/β interfacial energy γ = 140 mJ m– 2 was assessed from measurement of the time dependence of interlamellar distance during isothermal anneal.
Subject
Materials Chemistry,Metals and Alloys,Physical and Theoretical Chemistry,Condensed Matter Physics
Reference39 articles.
1. M. Avedesian, H. Baker: Magnesium and Magnesium Alloys, ASM Materials Park, OH (1999).
2. S.P. Kumar, S. Kumaran, T.S. Rao: Mater. Sci. Technol. 20 (2004) 835.
3. L.M. Klinger, Y.J.M. Brechet, G.R. Purdy: Acta Mater. 45 (1997) 5005.
4. D. Duly, Y. Brechet, B. Chenal: Acta Metall. Mater. 40 (1992) 2289.
5. P. Zhang, W. Blum: Z. Metallkd. 94 (2003) 716.